Over the past decade, degradation and power loss have been observed in PV modules resulting from the stress exerted by system voltage bias. This is due in part to qualification tests and standards that do not adequately evaluate for the durability of modules to the long-term effects of high voltage bias experienced in fielded arrays. High voltage can lead to module degradation by multiple mechanisms. The extent of the voltage bias degradation is linked to the leakage current or coulombs passed from the silicon active layer through the encapsulant and glass to the grounded module frame, which can be experimentally determined; however, competing processes make the effect non-linear and history-dependent. Appropriate testing methods and stress levels are described that demonstrate module durability to system voltage potentialinduced degradation (PID) mechanisms. This information, along with outdoor testing that is in progress, is used to estimate the acceleration factors needed to evaluate the durability of modules to system voltage stress. Na-rich precipitates are observed on the cell surface after stressing the module to induce PID in damp heat with negative bias applied to the active layer.

本帖子中包含更多资源

您需要 登录 才可以下载或查看,没有帐号?马上注册

分享到: QQ空间QQ空间 腾讯微博腾讯微博 腾讯朋友腾讯朋友
收藏收藏0
追逐太阳,追逐梦想!让我们一起努力,让光伏应用变的更简单!
QQ:24618879     E-mail:isunlicai@126.com
指尖的光伏 · 微信公众号:Solar-Research
回复

使用道具 举报

您需要登录后才可以回帖 登录 | 马上注册

 

领跑者创新论坛公众号二维码
回顶部